Low Viscosity, as reported by Dr. Spurr

Provides excellent penetration for embedding biological tissues and rapid infiltration. Easy to prepare. The hardness is adjusted by changing the proportion of the flexibilizer (DER 736). The blocks have good trimming and sectioning qualities. Thin sections are tough under the electron beam.
Spurr, A.R., (1969) J. Ultrastruct. Res. 26, 31-42

REF: D14300 Categories: ,

Description

D14300 Kit consists of :
450 ml NSA MSDS
225 ml ERL 4221 MSDS
225 ml DER 736 MSDS
25 ml DMAE MSDS

Technical Tip :_Low Viscosity Kit Formation with ERL 4221

 